Publication: Corrugated stainless steels embedded in mortar for 9 years: corrosion results of non-carbonated, chloride-contaminated samples
dc.affiliation.dpto | UC3M. Departamento de Ciencia e Ingeniería de Materiales e Ingeniería Química | es |
dc.affiliation.grupoinv | UC3M. Grupo de Investigación: Comportamiento en Servicio de Materiales | es |
dc.contributor.author | Bautista Arija, María Asunción | |
dc.contributor.author | Paredes, E. C. | |
dc.contributor.author | Velasco López, Francisco Javier | |
dc.contributor.author | Álvarez, S. M. | |
dc.date.accessioned | 2016-05-13T11:42:09Z | |
dc.date.issued | 2015-09-15 | |
dc.description.abstract | Mortar samples reinforced with 5 different corrugated stainless steels were tested for 9 years in 2 different conditions: partial immersion (PI) in 3.5% NaCl, and chloride addition to the mortar and exposure to high relative humidity (HRH). The monitoring during the exposures was carried out with corrosion potential (E-corr) and electrochemical impedance spectroscopy (EIS) measurements. A year before finishing (after 8 years of exposure), the reinforced mortar samples were anodically polarised to obtain more information about the pitting resistance of the passive layers formed under the different conditions. The last year of exposure was established to study the progress or repassivation of the pits. The PI is the most aggressive testing condition and it causes low-intensity corrosion in S20430 austenitic stainless steel after 7 years of exposure. The S32205 duplex stainless steel shows very good corrosion behaviour | en |
dc.description.sponsorship | The present work was funded by the Spanish Ministry of Science and Innovation through the Project reference BIA2007 66491 C02 02. | en |
dc.format.extent | 10 | es |
dc.format.mimetype | application/pdf | |
dc.identifier.bibliographicCitation | Construction and building materials 93 (2015), pp. 350-359 | en |
dc.identifier.doi | 10.1016/j.conbuildmat.2015.04.060 | |
dc.identifier.issn | 0950-0618 | |
dc.identifier.publicationfirstpage | 350 | es |
dc.identifier.publicationlastpage | 359 | es |
dc.identifier.publicationtitle | Construction and building materials | en |
dc.identifier.publicationvolume | 93 | es |
dc.identifier.uri | https://hdl.handle.net/10016/22970 | |
dc.identifier.uxxi | AR/0000017160 | |
dc.language.iso | eng | en |
dc.publisher | Elsevier Ltd. | es |
dc.relation.ispartof | http://hdl.handle.net/10016/22979 | |
dc.relation.projectID | Gobierno de España. BIA2007 66491 C02 02 | es |
dc.relation.publisherversion | http://dx.doi.org/10.1016/j.conbuildmat.2015.04.060 | es |
dc.rights | © 2015 Elsevier Ltd. | es |
dc.rights | Atribución–Nocomercial–Sinderivadas 3.0 España | * |
dc.rights.accessRights | open access | en |
dc.rights.uri | http://creativecommons.org/licenses/by-nc-nd/3.0/es/ | * |
dc.subject.eciencia | Materiales | es |
dc.subject.other | Stainless steel | en |
dc.subject.other | Steel reinforced mortar | en |
dc.subject.other | EIS | en |
dc.subject.other | Polarisation | en |
dc.subject.other | Passivity | en |
dc.subject.other | Pitting corrosion | en |
dc.title | Corrugated stainless steels embedded in mortar for 9 years: corrosion results of non-carbonated, chloride-contaminated samples | en |
dc.type | research article | * |
dc.type.hasVersion | AM | * |
dspace.entity.type | Publication |
Files
Original bundle
1 - 1 of 1